高品質3Dグラフェンフォーム(サイズカスタマイズ可能)
はじめに
The 3D Graphene Foam is made via chemical vapor deposition (CVD) processing. In course of CVD fabrication of graphene hydrogen and methane gases are introduced into a furnace that heats to 1000° Celsius. In the furnace is a nickel or copper film which captures a mono or multi-layer or graphene as the furnace is heated and the methane decomposes.
Advantages
- It has good conductivity and is an excellent light porous conductive carrier.
- On this substrate, we can grow a variety of oxide and hydroxide nanoarrays such as nickel oxide, cobalt oxide, cobalt trioxide, ferric oxide, cobalt hydroxide, nickel hydroxide, tungsten oxide, vanadium oxide, titanium oxide and so on.
仕様
| Sample size | 100*100mm (can be customized) |
| 厚さ | 1.2 mm-1.6mm |
| Density | 4 mg/cm3 |
| Pore Size | 580 microns |
| Packing | in sealed membrane box |
| 表面密度 | 0.5-0.9 mg/cm2. |
| Size of branches | 50-200 microns |
| Characteristic of large aperture | 200-500 microns. |
| Thermal conductivity | >6w/(m2k) |
| Standard PPI value | 110 |
寸法
| 0.1mm*200mm*300mm | 0.2mm*200mm*300mm | 0.3mm*200mm*300mm |
| 0.4mm*200mm*300mm | 0.5mm×200mm×300mm | 0.6mm*200mm*300mm |
| 0.7mm×200mm×300mm | 0.8mm×200mm×300mm | 0.9mm*200mm*300mm |
| 1mm×200mm×300mm | 1.6mm*20mm*300mm | サイズはカスタマイズ可能です |